Your Location : Home > TPE, TPR injection molding process
TPE, TPR injection molding process
Release Date : 2019/8/23 20:44:22  Click Volume : 6165
First, it must be dry before injection molding. Generally, it is hopper type drying 70~80°C/2h or tray drying 80~100°C/1h. For the drying of the tray, it should be noted that the thickness of the layer is generally not more than 50 mm. Tray drying is recommended. If there is foaming on the surface of the injected strip, or the strip is cut, and there is a cavity inside, or the surface of the product is scattered with silver, it can be determined that the TPE/TPR raw material has too much water content.

Second, try to use low temperature injection molding. Under the premise of ensuring the quality of plasticization, the extrusion temperature is reduced as much as possible, and the injection pressure and screw rotation speed are used to reduce the melt viscosity to achieve the purpose of improving fluidity. When the surface of the strip injected from the nozzle is smooth and bright, the plasticization quality is good. If the strip injected from the nozzle is very bright, it can be determined that the barrel temperature can also be lowered. Try to use low temperature injection molding to reduce cooling time and increase customer productivity.

Third, the upper parabolic temperature setting. The middle temperature of the screw is the highest, the feeding section is slightly lower, and the nozzle is slightly lower. Typical temperatures are set at 150-170 ° C (feed), 170-180 ° C (middle), 190-200 ° C (front), 180 ° C (nozzle). This temperature setting is only used as reference data. The specific temperature can be adjusted according to the specific physical properties of different TPE and TPR materials. If the content of the product is found to be bulging (the gas is contained inside), the gate is easily broken when the mold is released, and the adjustment can be made with reference to the second.

Fourth, the pressure holding pressure is as small as possible. Generally, the holding pressure is smaller than the injection pressure. The holding time can be determined by weighing the product, and the weight of the product is no longer increased, or the shrinkage mark accepted by the customer. If it is found that the gate is easy to break when demoulding, and the second can not be effective, it should be feasible to reduce the holding pressure.

5. If it is a few levels of injection, the speed is slow to fast. Because of this, the gas inside the mold is easily discharged. If there is gas inside the product (internal bulging), or there is a dent, the use of 訣竅2 is invalid, this method can be used to adjust.
主站蜘蛛池模板: 国产一区mp4| 成年黄网站18禁免费| 国产片A片永久免费观看| 无毒的黄色网站| 亚洲国产丝袜精品一区杨幂| 和离后我被太子娇养了免费阅读| 青草视频在哪| 好紧好爽再浪一点bl双性| 国产美女精品自在线拍| 和夜狼直播类似的app| 国产日韩在线视看高清视频手机| 嗯啊真粗…bl纯肉| 好男人神马社区| yy11111111少妇电影院光屁股| 鬼父在线观看三国影院| 爱综合色av| 调教踩踏论坛| 影院-精品影视在线看| 五月综合六月丁香| 男生下面伸进女人下面的视频 | 好男人视频免费高清在线观看| 日本肥婆bbwhd| 中国熟妇人妻videos| 国产亚洲精品免费观看视频| 国内如何浏览PROUMB| 国产青娱乐AV| 日本十八禁漫画彩漫| xxjjyy| mm1313亚洲精品| 海贼王在线高清免费观看| 曰本av电影手机在线观看| 成本人片无码中文字慕免费| 国产男同志CHINA69| 亚洲国产精品无码中文字导航| 国色天香社区在线观看高清| 撕开老师丝袜| 杨门十二寡妇艳史| 广州杀人王之人皮日记| 美女sssav| 综合无码免费| 久久久婷婷五月综合色| To Top